evolutionm.net - Home of the Lancer Evolution
Home Features Community Marketplace Registry Garage

Go Back   evolutionm.net > Lancer Evolution 1-9 Forums > Evo Advanced > Interior/Exterior/Electrical
New! Use your Facebook, Google, AIM & Yahoo accounts to securely log into this site, click logo to login  

Welcome to EvolutionM.net!
Welcome to EvolutionM.net.

You are currently viewing our forum as a guest, which gives you limited access to view most discussions and access our other features. By joining our community, at no cost, you will have access to post topics, communicate privately with other members (PM), respond to polls, upload content and access many other special features. Registration is free, fast and simple, so please join our community today!


Reply
 
Thread Tools
Old Jul 2, 2009, 11:28 AM   #1
Evolving Member
Personal Sales Rating: (7)
 
Join Date: Sep 2008
Location: ny/ct
Posts: 313

Drives: Evolution IX.

Can someone help me weld a crack in my front fender that i got from rolling them aggr

Can someone help me weld a crack in my front fenders that i got from rolling them aggressively. I am willing to pay money also.
Offline
 
Reply With Quote
Old Jul 2, 2009, 11:43 AM   #2
Evolved Member
Personal Sales Rating: (5)
 
Join Date: Jul 2006
Location: Denton, Tx
Posts: 535

Drives: Blue 2004 Evo, 1969 Datsun 2000 roadster.

You need someone to braze it as that metal is thin. You can likely get someone locally to do the work. Just when you say weld and fender folks may not be too willing.
Offline
 
Reply With Quote
Reply

Tags
fast, weld

Thread Tools

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are On
Refbacks are Off

 



All times are GMT -7. The time now is 12:56 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Content Relevant URLs by vBSEO 3.2.0